Problem:
Black / Brown Specks or deposits are visible on the surface of the moulding, normally caused by contamination or degradation of the material.
Solution:
- Reduce the temperature of the polymer melt.
- Reduce the screw speed and/or the back pressure.
- Clean the moulding machine thoroughly - full purge.
- Check for any impurities, leaks or dirt deposits in the feed stock hopper supply.
- Check the shot weight. The entire shot weight should not be less than 10-20 % of the maximum capacity of the machine.
- Check compatibility of pigment or masterbatch with the base polymer.
- Reduce the time in which the material is openly exposed to the ambient conditions.